Problem: Installing filled thermoplastic materials over metallic fasteners for low observable coating applications is a slow process that often results in poor material adhesion.

Solution: SMRC developed a laser-based handheld tool to install these materials in under 10 seconds per fastener with repeatable quality and performance.